Everything about Animal Glue totally explained
Image:Knochenleim Granulat.jpg|Animal glue, granules
Image:Cold glue.jpg|Hide glue at room temperature
Image:Hot glue.jpg|Hot hide glue
An
animal glue is an
adhesive that's created by prolonged boiling of
animal connective tissue.
Stereotypically, the animal in question is a
horse, and horses that are put down are often said to have been sent to the "glue factory"; this may be literally true.
These
protein colloid glues are formed through
hydrolysis of the
collagen from skins, bones, tendons, and other tissues, similar to
gelatin. The word "collagen" itself derives from
Greek kolla, glue. These proteins form a molecular bond with the glued object.
Types and uses
Animal glue was the most common woodworking glue for thousands of years until the advent of synthetic glues such as PVA and other resin glues in the 20th century. Today it's used primarily in specialty applications such as
lutherie,
pipe organ building, and antique restoration. Glass artists take advantage of hide glue's ability to bond with glass, applying hide glue to glass. As the glue hardens it shrinks, chipping the glass.
It has several advantages and disadvantages compared to other glues. The glue is applied hot, typically with a
brush or
spatula; it's kept hot in a
glue pot. Most animal glues are
soluble in
water, useful for
joints which may at some time need to be separated.
Alcohol is sometimes applied to such joints to dehydrate the glue, making it more brittle and easier to crack apart.
Specific types include
hide glue,
bone glue,
fish glue,
rabbit skin glue.
Hide glue
Hide glue is used in woodworking. It may be supplied as granules, flakes, or flat sheets, which have an indefinite
shelf life if kept dry. It is dissolved in water, heated and applied warm, typically around 140°
F. Warmer temperatures will quickly destroy the strength of most hide glues, so maintaining this temperature is critical. Commercial glue pots, simple water baths or double boilers may be used to keep the glue hot while in use. As hide glue cools, it gels quickly. At room temperature, prepared hide glue has the consistency of stiff
gelatin, which is in fact a similar composition. Gelled hide glue doesn't have significant strength, so it's vital to apply the glue, fit the pieces, and hold them steady before the glue temperature drops much below 120°F. All glues have an
open time, the amount of time the glue remains liquid and workable. Joining parts after the open time is expired results in a weak bond. Hide glue's open time is usually a minute or less. In practice, this often means having to heat the pieces to be glued, and gluing in a very warm room, though these steps can be dispensed with if the glue and clamp operation can be carried out quickly.
Where hide glue is in occasional use, excess glue may be held in a freezer, to prevent spoilage from the growth of
microorganisms.
Joints to be glued with hide glue must fit perfectly, as it has poor gap-filling properties.
Hide glue that's liquid at room temperature is also possible through the addition of urea. An example of this type of mixture is Old Brown Glue, created by W. Patrick Edwards, the director of the American School of French Marquetry. In stress tests performed by Mark Schofield of Fine Woodworking Magazine, liquid hide glue compared favourably to hot hide glue in average strength of bond.
Properties
This significant disadvantage to using hide glue is offset by several advantages. Hide glue joints are reversible and repairable. Recently glued joints will release easily with the application of heat and steam. Hide glue sticks to itself, so the repairer can apply new hide glue to the joint and reclamp it. In contrast, PVA glues don't adhere to themselves once they're cured, so a successful repair requires removal of the old glue first - which usually requires removing some of the material being glued.
Hide glue creates a somewhat brittle joint, so a strong shock will often cause a very clean break along the joint. In contrast, a joint glued with PVA will usually break the surrounding material, creating an irregular, difficult to repair break. This brittleness is taken advantage of by instrument makers. For example, instruments in the
violin family require periodic disassembly for repairs and maintenance. The top of a violin is easily removed by prying a palette knife between the top and ribs, and running it all around the joint. The brittleness allows the top to be removed, often without significant damage to the wood. Regluing the top only requires applying new hot hide glue to the joint. If the violin top was glued on with PVA glue, removing the top would require heat and steam to disassemble the joint (causing damage to the varnish), then wood would have to be removed from the joint to ensure no cured PVA glue was remaining before regluing the top.
Hide glue also functions as its own clamp. Once the glue begins to gel, it pulls the joint together. Violin makers may glue the center seams of top and back plates together using a
rubbed joint rather than using
clamps. This technique involves coating half of the joint with hot hide glue, and then rubbing the other half against the joint until the hide glue starts to gel, at which point the glue becomes tacky. At this point the plate is set aside without clamps, and the hide glue pulls the joint together as it hardens.
Hide glue regains its working properties after cooling if it's reheated. This property can be used when the glue's open time doesn't allow the joint to be glued normally. For example, a cello maker may not be able to glue and clamp a top to the instrument's ribs in the short one minute open time available. Instead, the builder will lay a bead of glue along the ribs, and allow it to cool. The top is then clamped to the ribs. Moving a few inches at a time, the maker inserts a heated palette knife into the joint, heating the glue. When the glue is liquefied, the palette knife is removed, and the glue cools, creating a bond. A similar process can be used to glue veneers to a substrate. The veneer and/or the substrate is coated with hot hide glue. Once the glue is cold, the veneer is positioned on the substrate. A hot object, such as a clothes iron is applied to the veneer, liquefying the underlying glue. When the iron is removed, the glue cools, bonding the veneer to the substrate.
Hide glue joints don't creep under loads. PVA glues create plastic joints, which will creep over time if heavy loads are applied to them.
Hide glue is supplied in many different gram strengths, each better suited to specific applications. Instrument and cabinet builders will use a range from 120-200 gram strength. Some hide glues are sold without the gram strength specified. Experienced users avoid this glue as the glue may be too weak or strong for the expected application.
Hoof glue
Hoof glue is also used today in woodworking, specifically cabinetry.
Rabbit-skin glue
Rabbit-skin glue is used in the
sizing or priming of
oil painters' canvases.
History
Nearly 5,000 years ago, the
Egyptians were using hide glue for their
furniture adhesive. This is proven by hairs found in
Pharaoh's
tombs and by stone carvings depicting the process of gluing different woods. Evidence exists that the
Sumerians also used glue before the
Egyptians did.
Further Information
Get more info on 'Animal Glue'.
|
External Link Exchanges
Do you know how hard it is to get a link from a large encyclopaedia? Well we're different and will prove it. To get a link from us just add the following HTML to your site on a relevant page:
<a href="http://animal_glue.totallyexplained.com">Animal glue Totally Explained</a>
Then simply click through this link from your web page. Our crawlers will verify your link, extract the title of your web page and instantly add a link back to it. If you like you can remove the words Totally Explained and embed the link in article text.
As long as your link remains in place, we'll keep our link to you right here. Please play fair - our crawlers are watching. Your site must be closely related to this one's topic. Any kind of spamming, dubious practises or removing the link will result in your link from us being dropped and, potentially, your whole site being banned. |